Add to Cart
C35 butt weld fitting 1.0501 Weld butt fittings ASME B16.9 Seamless Steel fittings
Grade : | C35 butt weld fitting | |||
Number: | 1.0501 weld butt fittings | |||
Classification: | Non-alloy quality steel | |||
Standard: |
|
Cr + Mo + Ni = max 0.63 |
C | Si | Mn | Ni | P | S | Cr | Mo |
0.32 - 0.39 | max 0.4 | 0.5 - 0.8 | max 0.4 | max 0.045 | max 0.045 | max 0.4 | max 0.1 |
Nominal thickness (mm): | to 16 | 16 - 100 | 100 - 250 | 250 - 500 | 500 - 1000 |
Rm - Tensile strength (MPa) (+N) | 550 | 520 | 500 | 480 | 470 |
Nominal thickness (mm): | 5 - 10 | 10 - 16 | 16 - 40 | 40 - 63 | 63 - 100 |
Rm - Tensile strength (MPa) (+C) | 650-1000 | 600-950 | 580-880 | 550-840 | 520-800
|
Nominal thickness(mm): | to 16 | 16 - 100 | 100 - 250 | 250 - 500 | 500 - 1000 |
Re - Upper yield strength or Rp0.2 - 0.2% proof strength (MPa) (+N) | 300 | 270 | 245 | 220 | 210 |
Nominal thickness(mm): | 5 - 10 | 10 - 16 | 16 - 40 | 40 - 63 | 63 - 100 |
Rp0.2 0.2% proof strength (MPa) (+C) | 510 | 420 | 320 | 300 | 270 |
A - Min. elongation at fracture (%) transverse, (+N) | 15 |
Nominal thickness (mm): | 5 - 10 | 10 - 16 | 16 - 40 | 40 - 63 | 63 - 100 |
A - Min. elongation at fracture (%) (+C) | 6 | 7 | 8 | 9 | 9 |
Nominal thickness (mm): | to 16 | 16 - 100 | 100 - 250 |
A - Min. elongation Lo = 5,65 √ So (%) (+N) | 18 | 19 | 19 |
Brinell hardness (HBW): (+SH) | 154 - 207 |
Weldability: It can be welded quite well without any precautions. Hardenability: Low hardenability; core quenching in water till a diameter of 12-15 mm; as far as bigger diameters are concerned, it hardens only till a certain depth, inversely proportional to diameter, like all nonalloy steels with medium-high carbon content. |
EU EN | USA - | Germany DIN,WNr | Japan JIS | France AFNOR | England BS | Italy UNI | Spain UNE | China GB | Sweden SS | Poland PN | Czechia CSN | Austria ONORM | Russia GOST | Inter ISO | ||||||||||||||||||||||
C35 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|