Add to Cart
Grade : | X6CrNiNb18-10 | ||||||||||||||
Number: | 1.4550 | ||||||||||||||
Classification: | Austenitic stainless steel - special grade | ||||||||||||||
Density: | 7.9 g/cm ³ | ||||||||||||||
Standard: |
|
Nb = 10 * C to 1.0 Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. |
C | Si | Mn | Ni | P | S | Cr | Nb |
max 0.08 | max 1 | max 2 | 9 - 12 | max 0.045 | max 0.015 | 17 - 19 | max 1 |
Rm - Tensile strength (MPa) (+A) | 500-740 |
Rm - Tensile strength (MPa) (+AT) | 510-740 |
Rp0.2 0.2% proof strength (MPa) (+AT) | 205 |
Rp0.2 0.2% proof strength (MPa) (+A) | 200-240 |
KV - Impact energy (J) transverse, (+A) | +20° 60 | -196° 40 |
KV - Impact energy (J) longitud., (+A) | +20° 100 |
A - Min. elongation at fracture (%) (+A) | 30-40 |
A - Min. elongation at fracture (%) longitud., (+AT) | 35 |
Brinell hardness (HB): (+A) | 230 |
Brinell hardness (HB): (+AT) | 210 |
Resistance to intergranular corrosion: in the delivery condition - yes; in the sensitized condition - yes Steel shal not be applied at a metal temperature lower than -196 ° C |
EU EN | USA - | France AFNOR | England BS | Sweden SS | Russia GOST | |||||
X6CrNiNb18-10 |
|
|
|
|
|