Grade : | X1CrNiMoCuN20-18-7 | |||||||||||||
Number: | 1.4547 | |||||||||||||
Classification: | Austenitic stainless steel - special grade | |||||||||||||
Density: | 8 g/cm ³ | |||||||||||||
Standard: |
|
Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. |
C | Si | Mn | Ni | P | S | Cr | Mo | N | Cu |
max 0.02 | max 0.7 | max 1 | 17.5 - 18.5 | max 0.03 | max 0.01 | 19.5 - 20.5 | 6 - 7 | 0.18 - 0.25 | 0.5 - 1 |
Rm - Tensile strength (MPa) (+A) | 650-850 |
Rm - Tensile strength (MPa) (+AT) | 650-850 |
Rp0.2 0.2% proof strength (MPa) (+AT) | 300 |
Rp0.2 0.2% proof strength (MPa) (+A) | 300-340 |
KV - Impact energy (J) transverse, (+A) | +20° 60 | -196° 60 |
KV - Impact energy (J) longitud., (+A) | +20° 100 |
A - Min. elongation at fracture (%) (+A) | 30-40 |
A - Min. elongation at fracture (%) transverse, (+AT) | 30 |
A - Min. elongation at fracture (%) longitud., (+AT) | 35 |
Brinell hardness (HB): (+A) | 260 |
Brinell hardness (HB): (+AT) | 220 |
Resistance to intergranular corrosion: in the delivery condition - yes; in the sensitized condition - yes Steel shal not be applied at a metal temperature lower than -196 ° C |
EU EN | USA - | Sweden SS | ||
X1CrNiMoCuN20-18-7 |
|
|