Grade : | S275J0H | ||
Number: | 1.0149 | ||
Classification: | Non-alloy structural steel | ||
Standard: |
|
Method of deoxidation FN = rimming steels not permitted C < 0.2 for thickness =< 40 mm, CEV < 0.41 / 0.48 for thickness 16 / 65 mm |
C | Mn | P | S | N |
max 0.22 | max 1.5 | max 0.035 | max 0.035 | max 0.009 |
Nominal thickness (mm): | to 3 | 3 - 100 | 100 - 120 |
Rm - Tensile strength (MPa) | 430-580 | 410-560 | 400-540 |
Nominal thickness (mm): | to 16 | 16 - 40 | 40 - 63 | 63 - 80 | 80 - 100 | 100 - 120 |
ReH - Minimum yield strength (MPa) | 275 | 265 | 255 | 245 | 235 | 225 |
KV - Impact energy (J) | 0° 27 |
Nominal thickness (mm): | to 40 | 40 - 63 | 63 - 100 | 100 - 120 |
A - Min. elongation at fracture (%) longitud., | 23 | 22 | 21 | 19 |